Mechanical Properties Metric English Comments
Flexural Strength 24.8 MPa
3600 psi
ASTM D955-89
Multibase Multi-Flex® TPO D 5308-20 BLK
Glass reinforced TOP with improved stiffness and retention of low temperature resistance.Data provided by Multibase.
Flexural Strength 24.8 MPa
3600 psi
ASTM D790-95
Multibase Multi-Pro® 0710 C Brown Polypropylene
Data provided by Multibase.
Flexural Strength 24.8 MPa
3600 psi
ASTM D790
PolyOne Maxxam™ PPC-20C Nat Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Strength 24.8 MPa
3600 psi
ASTM D790
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet)
Flexural Strength 24.8 MPa
3600 psi
ASTM D790
Chase Plastics CP Pryme® N300STL (COND, 50% RH) Nylon 6 (Utility Grade), Super Toughened, Internally Lubricated
Information provided by Chase Plastics.
Flexural Strength 24.8 MPa
3600 psi
ASTM D790
Ensinger XP-130 Compression Molded PI Compound, 30% PTFE Filled
The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability..