Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 20.69 MPa | >= 3001 psi | ASTM D638-95 |
Multibase Multi-Flex® TPO D 5308-20 BLK Glass reinforced TOP with improved stiffness and retention of low temperature resistance.Data provided by Multibase. |