Material Notes:
Ash is 14%. The moisture content is 0.05%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.9987 g/cc
0.03608 lb/in³
ASTM D792
Melt Flow 16 g/10 min
16 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore D 54.5
54.5
10 sec; ASTM D-2240
Tensile Strength, Ultimate 11.4 MPa
1650 psi
ASTM D638
Elongation at Break 710 %
710 %
ASTM D638
Flexural Strength 8.30 MPa
1200 psi
ASTM D790
Flexural Modulus 0.272 GPa
39.5 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 70.0 kN/m
399 pli
ASTM D624
Users viewing this material also viewed the following: