Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 8.30 MPa | 1200 psi | ASTM D790 |
Multibase Multi-Flex® TPE D 4112 BLK Ash is 14%. The moisture content is 0.05%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Strength | 8.30 - 10.3 MPa | 1200 - 1490 psi | |
Ceradyne Thermo-Sil® Castable 120 Fused Silica Fused Silica is an excellent thermal insulator with an extremely low coefficient of thermal expansion. It is excellent for thermal shock applications. The key characteristics of this material are:Hi.. |