Polymer Property : Flexural Modulus = 0.272 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.272 GPa
39.5 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE D 4112 BLK
Ash is 14%. The moisture content is 0.05%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Flexural Modulus 0.272 GPa
39.5 ksi
ASTM D790
Teknor Apex Telcar® TL-1182A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..