Adamas Adalon® 301 PTFE, 10% Graphite

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Adamas
Trade Name Adalon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Adamas Adalon® 301 PTFE, 10% Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Adamas, HPM
Physical Properties Metric English Comments
Specific Gravity 2.14 - 2.16 g/cc
2.14 - 2.16 g/cc
ASTM D792
Deformation 5.0 - 7.5 %
5.0 - 7.5 %
Permanent deformation after 24 hrs @ 23°C; ASTM D621
9.0 - 10.5 %
9.0 - 10.5 %
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 56 - 62
56 - 62
ASTM D2240
Tensile Strength at Break >= 19.0 MPa
>= 2760 psi
ASTM D4894
Elongation at Break >= 210 %
>= 210 %
ASTM D4894
Coefficient of Friction, Dynamic 0.080 - 0.10
0.080 - 0.10
ASTM D1894
Coefficient of Friction, Static 0.060 - 0.080
0.060 - 0.080
ASTM D1894
Thermal Properties Metric English Comments
Thermal Conductivity 0.390 W/m-K
2.71 BTU-in/hr-ft²-°F
ASTM C 177
Melting Point 327 °C
621 °F
DSC
Maximum Service Temperature, Air 260 °C
500 °F
DSC
Minimum Service Temperature, Air -180 °C
-292 °F
DSC
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
ASTM D257
Surface Resistance 1.00e+9 ohm
1.00e+9 ohm
ASTM D257