Multibase Multi-Flex® TPE A 4002 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 4002 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-Flex® A 4002 is based on Shell's Kraton G polymer and is suitable for soft touch applications for the automotive industry. It exhibits excellent paintibility adhesion. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min
4.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
10 sec; ASTM D-2240
Tensile Strength, Ultimate 4.80 MPa
696 psi
ASTM D412
Elongation at Break 1400 %
1400 %
ASTM D412
Flexural Modulus 0.0117 GPa
1.70 ksi
method 1, Proc.B; ASTM D-790
Tear Strength 26.6 kN/m
152 pli
ASTM D624