Tensile Strength, Ultimate 8.17 MPa
1180 psi
ASTM D412
Multibase Multi-Flex® TPE A 7101 BLK
Ash is 36.2%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tensile Strength, Ultimate 8.14 MPa
1180 psi
Dow Corning SILASTIC® Q7-4535 BIOMEDICAL GRADE ETR ELASTOMER
One-part, enhanced tear-resistant silicone elastomers; uncatalyzed (customer selects peroxide catalyst) elastomer materials designed for compounding into elastomer for part fabrication and medical d..
Tensile Strength, Ultimate 8.135 MPa
1180 psi
After 7 days at 100oC; ASTM D412 ISO 37
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6080NC/BK have excellent soft touc..
Tensile Strength, Ultimate 8.135 MPa
1180 psi
After 7 days at 70°C; ASTM D412 ISO 37
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6080NC/BK have excellent soft touc..
Copyright © lookpolymers.com All Rights Reserved