Multibase Multi-Flex® TEA 4001-65 TPO Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TEA 4001-65 TPO Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.982 g/cc
0.982 g/cc
ASTM 792
Melt Flow 39.1 g/10 min

@Load 2.16 kg,
Temperature 230 °C
39.1 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
10 seconds; ASTM D2240
Tensile Strength, Yield 12.1 MPa
1750 psi
Elastic; ASTM D412
Elongation at Break 890 %
890 %
ASTM D638
Tear Strength 33.3 kN/m
190 pli
ASTM D624
Processing Properties Metric English Comments
Middle Barrel Temperature 193 °C
380 °F
Front Barrel Temperature 204 °C
400 °F
Nozzle Temperature 210 °C
410 °F
Mold Temperature 35.0 °C
95.0 °F