Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.982 g/cc | 0.982 g/cc | ASTM D792 |
Polymax® Maxelast® P1885 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.982 g/cc | 0.982 g/cc | ASTM D792 |
Polymax® Maxelast® P2830 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.982 g/cc | 0.982 g/cc | ASTM D792 |
Polymax® Maxelast® P3830 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.982 g/cc | 0.982 g/cc | ASTM D792 |
Polymax® Maxelast® P3868H TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.982 g/cc | 0.982 g/cc | ASTM D792 |
Polymax® Maxelast® P3895 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.982 g/cc | 0.982 g/cc | ASTM D792 |
Polymax® Maxelast® P3897M TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Specific Gravity | 0.982 g/cc | 0.982 g/cc | ASTM 792 |
Multibase Multi-Flex® TEA 4001-65 TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Specific Gravity | 0.982 g/cc | 0.982 g/cc | ASTM 792 |
Multibase Multi-Flex® A 9002 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Specific Gravity | 0.982 g/cc | 0.982 g/cc | |
Esstech X-829-0050 Adhesive Monomer PMGDM, 50% (w/w) Solution in Acetone, C32H34O16 Pyromellitic glycerol dimethacrylate or PMGDM is an excellent liquid adhesive system. Applications exist in both the dental and cosmetic industry. Its' four methacrylate groups help to incorporate i.. |