Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.1 MPa
1760 psi
ASTM D412
Polymax® Maxelast® A9960 TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Strength, Yield 12.1 MPa
1760 psi
ASTM D412
Polymax® Maxelast® A9960C TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Strength, Yield 12.1 MPa
1760 psi
ASTM D412
Polymax® Maxelast® A9970H TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D412
Precision Polymer Engineering V75B Fluoroelastomer Compound
Fluoroelastomer Rubber, 66-75 °IRHD. Copolymer of vinylidene fluoride and hexafluoropropylene. To meet ASTM D2000 line call-out: M2HK710, A1-10, B37, B38, EF31, EO78, F14, Z1, where Z1 = compressi..
Tensile Strength, Yield 12.1 MPa
1750 psi
chs 20 in/min; ASTM D412
Network Polymers Softflex® 6500
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Tensile Strength, Yield 12.1 MPa
1760 psi
ASTM D638
Entec Hypel® PELLD20/.925 LLDPE  (discontinued **)
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Tensile Strength, Yield 12.1 MPa
1750 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 12.1 MPa
1760 psi
Elastic; ASTM D412
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot..
Tensile Strength, Yield 12.1 MPa
1750 psi
Elastic; ASTM D412
Multibase Multi-Flex® TEA 4001-65 TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Tensile Strength, Yield >= 12.1 MPa
>= 1750 psi
Stress at Elongation M100; ASTM D412 Method A
Seals Eastern 7130 Fluorocarbon-Elastomer
FKM specially for oil & gas service.Information provided by Seals Eastern, Inc.
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D412
Teknor Apex APEX® 1700-70 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met..
Tensile Strength, Yield 12.1 MPa
1760 psi
100%; ASTM D412
Teknor Apex APEX® 3090-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D412
Teknor Apex APEX® 90-A41R-65-NT Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Uses- Medical Applications, Tubing, Appearance-ClearForms-PelletsProcessing-ExtrusionInformation provided by..
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D412
Vicone High Performance Rubber VicoSeal™ 106C-BK High Performance EPDM Rubber
Information provided by Vicone
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Axiall 53080A Moldings & Extrusions Flexible PVC
General purpose molding grade compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Axiall 8740 Moldings & Extrusions Flexible PVC
General purpose extrusion compound recommended for use in weatherstrips, screen spline, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporatio..
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Axiall 8743 Moldings & Extrusions Flexible PVC
A high quality extrusion compound recommended for weatherstrips, extruded shapes and flexible gaskets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Axiall 8747 Moldings & Extrusions Flexible PVC
Economical general purpose molding and extrusion compound with good flex whitening resistance especially in darker colors.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation i..
Tensile Strength, Yield 12.1 MPa
1750 psi
2 in/min (50 mm/min); ASTM D638
Bapolene® 2272 Polyethylene, Injection Grade
Bapolene LL2272 is a high flow, narrow molecular weight distribution, linear low density polyethylene injection resin. This resin offers excellent stress cracking resistance, flex life, low tempera..
Tensile Strength, Yield 12.1 MPa
1750 psi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Suprex Clay Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
Tensile Strength, Yield 12.1 MPa
1750 psi
ASTM D-638
Axiall 46234B Flexible PVC
Injection molding compound designed for automotive encapsulation applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 12.1 MPa
1760 psi
9.8 in/min; ASTM D638
Teknor Apex Sinvicomp SFC 8000 Polyvinyl Chloride, Flexible
Availability: Asia Pacific Features: Foamable Uses: Footwear Forms: Pellets Processing Method: Injection MoldingInformation Provided by Teknor Apex