Material Notes:
Description: Pluracol® 726 polyol is a 3000 molecular weight propylene oxide adduct of glycerine. Originally designed as a slabstock foam polyol, Pluracol 726 has found wide acceptance in specialty non-foam polyurethane applications.Information provided by BASF
Physical Properties Metric English Comments
Density 0.977 g/cc

@Temperature 60.0 °C
0.0353 lb/in³

@Temperature 140 °F
0.992 g/cc

@Temperature 37.8 °C
0.0358 lb/in³

@Temperature 100 °F
1.00 g/cc

@Temperature 25.0 °C
0.0361 lb/in³

@Temperature 77.0 °F
Viscosity 110 cP

@Temperature 60.0 °C
110 cP

@Temperature 140 °F
210 cP

@Temperature 37.8 °C
210 cP

@Temperature 100 °F
420 cP

@Temperature 25.0 °C
420 cP

@Temperature 77.0 °F
Molecular Weight 3000 g/mol
3000 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.015
<= 0.015
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Color Clear Liquid
Composition Na & K
<5 ppm, STI 3038
Hydroxyl Number 56 - 59 mg KOH/g
STI 3007/3162