Mechanical Properties Metric English Comments
Flexural Modulus 0.414 GPa
60.0 ksi
1% Secant; ASTM D790
LyondellBasell Purell® PE3020D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding
Purell PE 3020 D is a low density polyethylene with high rigidity, good opticals and good chemical resistance. It is delivered in pellet form. Target markets are small blow molding including packagi..
Flexural Modulus 0.414 GPa
60.0 ksi
ASTM D790
Multibase Multi-Flex® D 4210 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, GoodStiffness, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation p..
Flexural Modulus 0.414 GPa
60.0 ksi
1% Secant; ASTM D790
Multibase Multi-Flex® 1047 Black TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Flexural Modulus 0.414 GPa
60.0 ksi
ASTM D790
Multibase Multi-Flex® 1047-0000 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI..
Flexural Modulus 0.414 GPa
60.0 ksi
ASTM D790
Techmer ES HiFill® TPU 0780
Availability: North AmericaForms: PelletsFeatures: High DensityInformation provided by TP Composites, Inc.
Flexural Modulus 0.414 GPa
60.0 ksi
ASTM D790
Teknor Apex Telcar® TL-1155B Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Flexural Modulus 0.414 GPa
60.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Flexural Modulus 0.414 GPa
60.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Flexural Modulus 0.414 GPa
60.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Flexural Modulus 0.414 GPa
60.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Flexural Modulus 0.414 GPa
60.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..
Flexural Modulus 0.414 GPa
60.0 ksi
ASTM D790
Ecomass® 4703ZG92 Filled Polyurethane
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsModerate Specific GravityFilled Polyurethane (TPU)FlexibleInformation provided by Technical Polymers
Flexural Modulus 0.414 GPa
60.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman CP810-01 Natural Linear, Low-Density Polyethylene
DescriptionCP 810-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP 810-01 meets the specifications contained in FDA..