Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.98 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM D792
3M Dyneon™ THV 500A Fluorothermoplastic  (discontinued **)
THV 500A is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of an agglomerate. As an agglomerate, it can be used for c..
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM D792
PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled  (disco
Information provided by PolyOne™ Corporation
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 584 Perfluoroelastomer
Greene Tweed’s Chemraz® 584, a cream-colored perfluoroelastomer, is a specialty compound formulated to outlast the most demanding chemical process applications. Because of its outstanding o..
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM 792
Multibase Multi-Flex® D 4210 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Noise DampingOzone Resistant Thermal Stability, GoodStiffness, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInformation p..
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM D297
Greene Tweed CHEMRAZ® 570 Perfluoroelastomer
Chemraz® 570, recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control is required, offers excellent perfor..
Specific Gravity 1.98 g/cc
1.98 g/cc
Silberline Silvex® 115-20-D
Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use ..
Specific Gravity 1.98 g/cc
1.98 g/cc
Silberline Silvex® 225-20-D
Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use ..
Specific Gravity 1.98 g/cc
1.98 g/cc
Silberline Sparkle Silvex® 755-20-D
Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
Specific Gravity 1.98 g/cc
1.98 g/cc
Silberline Sparkle Silvex® 760-20-D
Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
Specific Gravity 1.98 g/cc
1.98 g/cc
Silberline Sparkle Silvex® 795-20-D
Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
Specific Gravity 1.98 g/cc
1.98 g/cc
Silberline Sparkle Silvex® 885-20-D
Sparkle Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited ..
Specific Gravity 1.98 g/cc
1.98 g/cc
Silberline Silvex® 545-20-D
Silvex® D grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited for use ..
Specific Gravity 1.98 g/cc
1.98 g/cc
3M Dyneon™ PFE 60Z Perfluoroelastomer
Dyneon™ PFE 60 Z is a technically advanced peroxide curable perfluoroelastomer, designed to meet the challenges of demanding sealing applications. It’s fully fluorinated back bone structure provid..
Specific Gravity 1.98 g/cc
1.98 g/cc
ASTM D792
3M Dyneon™ THVP 2030GZ Fluorothermoplastic Granules
THVP 2030GZ is a very flexible, transparent fluoroplastic composed of fluorinated monomers. It is ideal for applications that require the good temperature, chemical and flame resistance of a fluorop..
Specific Gravity 1.98 g/cc
1.98 g/cc
Part B; TM R050-16
Resinlab® EP1200 Black Casting Resin
Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re..
Specific Gravity 1.98 g/cc
1.98 g/cc
BYK Cloisite® 30B Nanoclay
Cloisite® 30B is an additive for plastics to improve various plastic physical properties, such as reinforcement, HDT, CLTE and barrier. Information provided by Southern Clay ProductsSouthern Clay P..
Copyright © lookpolymers.com All Rights Reserved