Momentive Performance Materials TSE3221 Clear Adhesive Sealant, Non-Corrosive Flowable

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Adhesive/Sealant Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials TSE3221 Clear Adhesive Sealant, Non-Corrosive Flowable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part heat cure. Typical uses: General sealing, potting, and coating when visual clarity is needed.Data provided by the manufacturer, GE Silicones.GE Silicones became a part of Momentive Performance Materials in 2006.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 28
28
Tensile Strength, Ultimate 2.35 MPa
341 psi
Elongation at Break 290 %
290 %
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Electrical Properties Metric English Comments
Dielectric Constant 2.8
2.8
Dielectric Strength 21.0 kV/mm
533 kV/in
Processing Properties Metric English Comments
Processing Temperature 100 °C
212 °F
Cure time 3 hr at this temperature.