LATI Latishield 87/28-10A G/20 PC, Steel/Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Stainless Steel Fiber
Manufacturer LATI
Trade Name Latishield
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latishield 87/28-10A G/20 PC, Steel/Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMI shielding product based on Polycarbonate (PC). Steel fibers. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 5.10 GPa
740 ksi
Charpy Impact Unnotched 4.50 J/cm²
21.4 ft-lb/in²
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
Vicat Softening Point 150 °C

@Load 5.00 kg
302 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Volume Resistivity 1000 ohm-cm
1000 ohm-cm
Surface Resistance 100 ohm
100 ohm
Processing Properties Metric English Comments
Melt Temperature 275 - 320 °C
527 - 608 °F
Mold Temperature 80.0 - 110 °C
176 - 230 °F
Drying Temperature 110 - 130 °C
230 - 266 °F
Descriptive Properties Value Comments
Electromagnetic reflection 90 dB
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following: