Mechanical Properties Metric English Comments
Tensile Strength 5.50 MPa
798 psi
Solid Silicone Rubber Sheet
P & P Technology Silicone Sheet
Silicone sheet is FDA approved. Translucent sheet is FDA @ WRC approved. FDA Certificate No. 177.2600Information provided by P & P Technology
Tensile Strength 5.50 MPa
798 psi
ISO 37
Termopol Termoton® V2GA1065A TPV Compound
Termoton®V, TPV compounds with a dynamically cured EPDM phase closely dispersed in a polyolefin phase (PP). Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable;..
Tensile Strength 5.50 MPa
798 psi
Momentive Performance Materials Electro 170 Heat Cured Rubber - High Voltage Insulating
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta..
Tensile Strength 5.50 MPa

@Strain 100 %
798 psi

@Strain 100 %
ISO 37
BASF Elastollan 685 AU TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength 5.50 MPa
798 psi
100; ISO 37
BASF Elastollan SP 9213 TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tensile Strength >= 5.50 MPa
>= 798 psi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Tensile Strength 5.50 MPa
798 psi
100; ISO 37
BASF Elastollan 880 AN TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tensile Strength 5.50 MPa
798 psi
ISO 37
AlphaGary Evoprene™ 3273 Standard SBS Thermoplastic Elastomer Compound
Tensile Strength 5.50 MPa
798 psi
ISO 37
AlphaGary Evoprene™ 003 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Tensile Strength 5.50 MPa
798 psi
ISO 37
AlphaGary Evoprene™ Super G 947 SEBS Thermoplastic Elastomer
Evoprene™ Super G compounds are high performance styrene ethylene- butylene styrene based thermoplastic elastomers. Evoprene™ Super G has improved heat resistance and improved recovery properties..