Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 2.1 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.1 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 48.8 MPa
7080 psi
chs 2 in/min; ASTM D638
Flexural Modulus 2.301 GPa
333.7 ksi
chs 0.05 in/min; ASTM D790
Izod Impact, Notched 1.068 J/cm

@Thickness 3.17 mm
2.001 ft-lb/in

@Thickness 0.125 in
ASTM D256
Optical Properties Metric English Comments
Haze 4.2 %

@Thickness 3.00 mm
4.2 %

@Thickness 0.118 in
ASTM D1003
Transmission, Visible 88 %

@Thickness 3.00 mm
88 %

@Thickness 0.118 in
ASTM D1003