Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Micropol L7 Low density polyethylene rotational molding powder

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Micropol Limited
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Micropol L7 Low density polyethylene rotational molding powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Has a high gloss finish, and outstanding toughness. Information provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.916 g/cc
0.0331 lb/in³
ASTM D1505
Melt Flow 6.0 - 8.0 g/10 min
6.0 - 8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 12.5 MPa
1810 psi
ASTM D638-64T
Elongation at Break 500 %
500 %
50mm/min
Flexural Modulus 0.200 GPa
29.0 ksi
ASTM D760-66
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C
189 °F
ASTM D1525
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Users viewing this material also viewed the following: