Michelman® Michem® Guard 7140 Anionic dispersion of polyethylene wax

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Guard
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Guard 7140 Anionic dispersion of polyethylene wax.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Anionic dispersion of polyethylene waxUsage: Michem® Guard 7140 is a water-based, large particle emulsion which improves rub and abrasion resistance in pigmented coatings and semi-gloss coatings, inks and OPVs at very low addition rates; produces smooth satin finishes at 5-10% addition rates.Typical uses include: Inks and OPVs; Exterior wood and wood composites and Interior furniture and flooringInformation provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
Volatiles 59.5 - 60.5 %
59.5 - 60.5 %
pH 4.0 - 6.0
4.0 - 6.0
4.0 - 10
4.0 - 10
Recommended pH of system
Brookfield Viscosity <= 500 cP
<= 500 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance White liquid
Emulsifier Charge Anionic
Solids Type Polyethylene