Michelman® Michem® Guard 55 Nonionic polyethylene dispersion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Guard
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Guard 55 Nonionic polyethylene dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Nonionic polyethylene dispersionUsage: Michem® Guard 55 is a dispersion which provides mar and flatting properties when used as an additive in paint, coating, ink and graphic art formulations.Typical uses include: Inks and OPVs; Exterior wood and wood composites and Interior furniture and flooringFood Contact Information when manufactured in Belgium:FDA:175.105: Components of adhesives.176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
Volatiles 59.5 - 60.5 %
59.5 - 60.5 %
pH 2.0 - 12
2.0 - 12
Recommended pH of system
6.5 - 8.5
6.5 - 8.5
Brookfield Viscosity 500 - 5000 cP
500 - 5000 cP
Spindle # 4, rpm 60
Descriptive Properties Value Comments
Appearance White, free-flowing paste
Emulsifier Charge Nonionic
Solids Type Polyethylene