MetalTek Bearium® B-11 Bearing Bronze

Category Metal , Nonferrous Metal , Copper Alloy , Bronze
Manufacturer MetalTek
Trade Name Bearium®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek Bearium® B-11 Bearing Bronze.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Exceptional frictional properties as a result of uniformly dispersed microstructure constituents.Applications: Turbine thrust bearings, centrifuge bushings, shaft sleeves, and other severe duty, mission critical bearings and bushings. Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 60
60
500 kg
Tensile Strength, Ultimate >= 210 MPa
>= 30500 psi
Tensile Strength, Yield >= 110 MPa
>= 16000 psi
Elongation at Break >= 8.0 %
>= 8.0 %
Component Elements Properties Metric English Comments
Copper, Cu 70 %
70 %
Lead, Pb 18 %
18 %
Nickel, Ni 1.5 %
1.5 %
Tin, Sn 10 %
10 %