Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF)  (Unverified Data**)

Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Hylar® 301F Polyvinylidene Fluoride (PVDF)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Melt Viscosity - Polymer for Non-Architectural Dispersion CoatingsInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.76 g/cc
1.76 g/cc
ASTM D792
Water Absorption at Saturation 0.020 %
0.020 %
ASTM D570
Viscosity 3.00e+6 cP
3.00e+6 cP
232°C, 100 sec^-1; ASTM D3835
Thermal Properties Metric English Comments
Heat of Fusion 40.0 J/g
17.2 BTU/lb
ASTM D3418
44.0 J/g
18.9 BTU/lb
Crystallization Heat; ASTM D3418
Specific Heat Capacity 1.30 J/g-°C
0.311 BTU/lb-°F
ASTM D3418
Melting Point 160 °C
320 °F
ASTM D3418
Crystallization Temperature 124 °C
255 °F
Peak, DSC; ASTM D3418
Decomposition Temperature 375 °C
707 °F
1% Mass Loss, Air
410 °C
770 °F
1% Mass Loss, N2
Optical Properties Metric English Comments
Gloss 25 %
25 %
Gardner; 60°; ASTM D523
Descriptive Properties Value Comments
Availability Europe
North America
Dispersion 5.5
ASTM D1210; Hegman Grind
Features High Viscosity
Homopolymer
Forms Powder
Generic PVDF
Processing Method Coating
Uses Coating Applications