Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® NA206000 Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Extrusion Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® NA206000 Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsPETROTHENE NA 206-000 is an extrusion coating resin especially recommended for high-speed, light weight coating applications. The resin can be drawn to a 3 lb/ream coating weight at line speeds in excess of 1500 fpm with minimum neck-in and no edge weave. It is recommended for locker wraps, sugar pouches, industrial and multi-wall bags and laminations. Regulatory StatusNA 206-000 meets requirements of the Food and Drug Administration regulations 21 CFR 177.1520 and 21 CFR 176.170. These regulations (respectively) allow for the use of the olefin polymer in "…articles or components of articles intended for use in contact with food; "or as components of the uncoated or coated food-contact surface of paper and paperboard intended for use in producing, manufacturing, packaging, processing, preparing, treating, packing, transporting or holding aqueous and fatty food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesIt is recommended that a melt temperature of 590°-620°F be used for light-weight coating applications in conjunction with electrostatic, flame or chemical priming to insure good adhesion. The maximum recommended melt temperature for NA 206-000 is 625°F. For further suggestions, please contact your Equistar sales representative.Physical PropertiesThese are typical values and not to be construed as specific product limits.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D1505
Melt Flow 13.5 g/10 min
13.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ASTM D2240
Tensile Strength at Break 11.0 MPa
1600 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Stiffness 207 MPa
30000 psi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 84.0 °C
183 °F
ASTM D1525
Users viewing this material also viewed the following: