Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 13.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
13.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Plaskolite Optix® CA - 51 LL General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Melt Flow 13.5 g/10 min

@Load 5.00 kg,
Temperature 260 °C
13.5 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® CM5820 PC+ABS (Asia Pacific)
Cycoloy CM5820 resin is a Mineral Filled Non-FR PC+ABS blend with high impact, high modulus, good chemical resistance & improved surface aesthetic, designed for hand help device chassis that require..
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 260 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS
Color package may affect performance. PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance.
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 260 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® FXC630SK PC+ABS (Asia Pacific)
PC+ABS, ECO-conforming flame retardant with diamond sparkle appearance.
Melt Flow 13.5 g/10 min

@Load 5.00 kg,
Temperature 260 °C
13.5 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS
Automotive applications: High impact and ductility to -22F for interior trim and instrument panel applications.
Melt Flow 13.5 g/10 min

@Load 5.00 kg,
Temperature 260 °C
13.5 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS (Asia Pacific)
IP1000 is a high impact PC/ABS blend developed for the automotive instrument panel business.
Melt Flow 13.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
13.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Plaskolite West Optix® CA - 51 LL General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ineos H13G-00 Polypropylene Homopolymer  (discontinued **)
Formerly Amoco® 7444. Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Medical componentsComplies with FDA specification, Title 21, C..
Melt Flow 13.5 - 16.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
13.5 - 16.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Kazanorgsintez PC-015 Polycarbonate
Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of die-casting.Information Provided by Kazanorgsintez
Melt Flow 13.5 g/10 min
13.5 g/10 min
ASTM D1238
LyondellBasell Petrothene® NA206000 Low Density Polyethylene
ApplicationsPETROTHENE NA 206-000 is an extrusion coating resin especially recommended for high-speed, light weight coating applications. The resin can be drawn to a 3 lb/ream coating weight at lin..
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ineos H13M-00 Polypropylene Homopolymer
Grade H13M-00 is a general purpose polypropylene homopolymer for injection molding applications. It provides good long-term heat stability.Suggested fabrication methods: Injection moldingFeatures: ..
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
IRPC Polimaxx Polene 1196NN Polypropylene Compound
CHARACTERISTICS: POLYPROPYLENE HOMOPOLYMER UNREINFORCED, CONTAIN FLAME RETARDANT, UL 94 V-2 APPROVAL, HIGH IMPACT STRENGTHAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES
Melt Flow 13.5 g/10 min

@Load 6.60 kg,
Temperature 337 °C
13.5 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM 2212R PEI
20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Melt Flow 13.5 g/10 min

@Load 6.60 kg,
Temperature 337 °C
13.5 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
SABIC Innovative Plastics ULTEM 2212R PEI (Asia Pacific)
20% Milled glass filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.
Melt Flow 13.5 g/10 min

@Load 10.0 kg,
Temperature 250 °C
13.5 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR
Information provided by Samsung Cheil Industries.
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex ELEXAR® EL 8421 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Melt Flow 13.5 g/10 min

@Load 5.00 kg,
Temperature 280 °C
13.5 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS
Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 ..
Melt Flow 13.5 g/10 min

@Load 5.00 kg,
Temperature 280 °C
13.5 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Asia Pacific)
Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 ..
Melt Flow 13.5 g/10 min

@Load 5.00 kg,
Temperature 280 °C
13.5 g/10 min

@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an..
Melt Flow 13.5 g/10 min

@Load 10.0 kg,
Temperature 250 °C
13.5 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Samsung Cheil Industries Infino® NH-8310 MPPE, Glass Filled FR
Information provided by Samsung Cheil Industries.
Melt Flow 13.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
13.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Supreme Petrochem SP6432 9690 Medium Impact Polystyrene
Characteristics High flow Good toughness Available in various colors Processing Injection moldingApplications Air conditioner and cooler grills Refrigerator parts Washing machine components Mate..
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133
DSM Arnitel® VT3104 TPC-ET
Extrusion Grade
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 250 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 482 °F
cm³/10min; ISO 1133
DuPont Performance Polymers Crastin® HR5315HFS BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate with Improved Processing Crastin HR5315HFS is a 15% glass fiber reinforced moderatley toughened hydrolysis resistant polybutylene..
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Dow DT702 TPO
Dow Fascia TPO for Painted ApplicationsInformation provided by Dow
Melt Flow 13.5 g/10 min
13.5 g/10 min
ASTM D1238
Formosa Plastics Formolene® LH5214 Injection Molding HDPE  (discontinued **)
High Density Polyethylene for Injection Molding Applications Formolene® LH5214 meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of ..
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
DuPont Nucrel® 1214 Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinued
12 wt% Methacrylic Acid.Nucrel® 1214 is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment des..
Melt Flow 13.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ineos H13Z-00 Polypropylene Homopolymer  (discontinued **)
Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope..