Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (1.5 mil Film)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® GA503027 Linear Low Density Polyethylene (1.5 mil Film).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsGA 503 is a medium density, butene copolymer LLDPE resin with high draw for stiff, thin blown films. GA 503 contains an antioxidant package to minimize discoloration and eliminate die build-up. Other additive formulations may be available for your specific application. Contact your Equistar sales representative for additional information. Processing TechniquesGA 503 provides high output at low melt temperatures and without high pressure, high torque or shear-induced melt fracture. For improved drawdown without bubble breaks, GA 503 can be blended with LDPE. GA 503 can be blended with high performance LLDPE grades to reduce torque and horsepower requirements. Specific recommendations for type of resin and extrusion conditions can be made only when the end use, required properties and processing equipment are known. For further suggestions, please contact your Equistar sales representative. Regulatory StatusGA 503 series resins meet the requirements of the Food and Drug Administration regulation, 21 CFR 177.1520, Subpart C, Item 3.1. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food…" Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.Other Information1.5 Film thickness.Physical PropertiesTesting was performed on film produced at a 2.5:1 BUR, 360°F (182°C) melt temperature, using an 8" die with 0.025" die gap, at 150 lb/hr.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.925 g/cc
0.0334 lb/in³
ASTM D1505
Thickness 38.1 microns
1.50 mil
Melt Flow 3.5 g/10 min
3.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 690 %
690 %
ASTM D882
Film Elongation at Break, TD 740 %
740 %
ASTM D882
Elmendorf Tear Strength MD 100 g
100 g
ASTM D1922
Elmendorf Tear Strength TD 215 g
215 g
ASTM D1922
Dart Drop Test 110 g
0.243 lb
F<sub>50</sub>, Estimated from TEDD value of 0.3 ft-lbs. For standard dart and 26" drop height.; ASTM D1709
Film Tensile Strength at Break, MD 33.1 MPa
4800 psi
ASTM D882
Film Tensile Strength at Break, TD 23.4 MPa
3400 psi
ASTM D882
1% Secant Modulus, MD 307 MPa
44500 psi
ASTM D638
1% Secant Modulus, TD 314 MPa
45500 psi
ASTM D638
Optical Properties Metric English Comments
Haze 30 %
30 %
ASTM D1003
Gloss 25 %
25 %
ASTM D2457
Descriptive Properties Value Comments
Antiblock High
Slip High