Description: INDURE™ X210 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, and processability. Applications: Bumper fascias, cladding. Information provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay Engineered Polymers in 2008.
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
ASTM D792B
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
as molded; ISO 294
Melt Flow 42 g/10 min
42 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 24.0 MPa
3480 psi
50 mm/min; ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
80x10x4 mm specimen, 2 mm/min; ASTM D790
Thermal Properties Metric English Comments
CTE, linear 75.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
41.7 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM D696