Mechanical Properties Metric English Comments
Flexural Modulus 0.660 GPa
95.7 ksi
ASTM D790
Nylene® PX1719 Nylon 6
Dry as molded. Extrusion grade. Nylene PX1719HS is a heat stabilized, high impact, nylon 6 extrusion grade resin with a low flexural modulus. PX1719HS is ideally suited for extrusion of tubing and..
Flexural Modulus 0.660 GPa
95.7 ksi
3 pt. secant. ASTM D790
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin  (discontinued **)
Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In..
Flexural Modulus 0.660 GPa
95.7 ksi
3 pt. secant. ASTM D790
Chevron Phillips HiD® 9642 HDPE Sheeting Resin  (discontinued **)
Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain..
Flexural Modulus 0.660 - 1.47 GPa
95.7 - 213 ksi
Average value: 1.02 GPa Grade Count:10
Overview of materials for High Density Polyethylene (HDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max..
Flexural Modulus 0.660 GPa
95.7 ksi
ISO 178
LyondellBasell Hostacomâ„¢ RE-44AC Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ RE-44AC polypropylene TPO resin is a compounded product containing 25% minimum post-industrial or post-consumer recycled polypropylene and reactor grade thermoplastic ole..
Flexural Modulus 0.660 GPa
95.7 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR
LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Flexural Modulus 0.660 GPa
95.7 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR (Asia Pacific)
LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Flexural Modulus 0.660 GPa
95.7 ksi
ASTM D790
Goodfellow TPX® MX002O Polymethylpentene
This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi..
Flexural Modulus 0.660 GPa
95.7 ksi
2% Secant - 16:1 span:depth, 0.5 in/min; ASTM D-790
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE
Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre..
Copyright © lookpolymers.com All Rights Reserved