LyondellBasell Alathon® M6030 High Density Polyethylene

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Film Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® M6030 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON M 6030 is a medium molecular weight high density homopolymer with extremely low gel content. Typical applications for this resin are cast film, coextrusion and dry food packaging.Regulatory StatusM 6030 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing M 6030 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.Typical Extrusion ConditionsMelt Temperature- 390°F(199°C)This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 22.1 MPa
3200 psi
ASTM D822
Film Tensile Strength at Yield, TD 20.7 MPa
3000 psi
ASTM D822
Film Elongation at Break, MD 860 %
860 %
ASTM D822
Film Elongation at Break, TD 850 %
850 %
ASTM D822
Elmendorf Tear Strength MD 20 g
20 g
ASTM D1922
Elmendorf Tear Strength TD 500 g
500 g
ASTM D1922
1% Secant Modulus, MD 689 MPa
100000 psi
ASTM D822
1% Secant Modulus, TD 827 MPa
120000 psi
ASTM D822
Processing Properties Metric English Comments
Melt Temperature 199 °C
390 °F
Typical Extrusion