Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 20.7 MPa | 3000 psi | ASTM D822 |
LyondellBasell Alathon® M6030 High Density Polyethylene ApplicationsALATHON M 6030 is a medium molecular weight high density homopolymer with extremely low gel content. Typical applications for this resin are cast film, coextrusion and dry food packagin.. |
|||
Film Tensile Strength at Yield, TD | 20.7 MPa | 3000 psi | 10 in/min; ASTM D-882 |
Bapolene® 105F Low Density Polyethylene Film Resin Description: Bapolene LD105F is an unmodified low density polyethylene which extrudes into a low gloss high impact film. It contains antiblock additives and no slip additives. This product meets th.. |