Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 75.0 °C | 167 °F | TM R050-25 |
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | |
Lord Adhesives Thermosetâ„¢ LS 213-9 Unfilled Epoxy Encapsulant Lord LS 213-9 is a one component epoxy coating and impregnating compound featuring low viscosity, good moisture resistance and excellent dielectric properties. Typical applications include transform.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | |
Lucite International Elvacite ® 4026 Acrylic Resin Elvacite® 4026 is a solid acrylic bead resin which has been specially developed for use as a performance enhancing additive in a range of radiation (UV and EB) curable inks and coatings. These en.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Ultimate Tg |
Tra-Con Tra-Bond 2222 One-Part Surface Mount Epoxy Adhesive TRA-BOND 2222 is a solvent-free, one-part thixotropic, epoxy adhesive recommended for SMD (Surface Mount Device) bonding and sealing applications where its easy handling, high strength and superior .. |
|||
Glass Transition Temp, Tg | 75.0 - 80.0 °C | 167 - 176 °F | |
Master Bond Supreme 11AO Electrically Isolating Adhesive and Sealant Description: Master Bond Polymer System SURPEME 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Ultimate Tg |
Tra-Con Tra-Bond 9070D Filled Epoxy Adhesive TRA-BOND 9070D filled epoxy adhesive exhibits a low coefficient of expansion. Information provided by Tra-Con Inc. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® 46HF4130 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE250F3 Nylon 46-15% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE341 Nylon 46 (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE373 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW363 Nylon 46 (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | ASTM D1525 |
Eastman Eastar GN077 Copolyester, Natural Eastar Copolyester GN077 is an amorphous resin with good melt strength, chemical resistance, high clarity and gloss. It is an excellent choice for extrusion blow molding small to intermediate size c.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Dry)
(discontinued **) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Average value: 75.0 °C Grade Count:16 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 - 275 °C | 167 - 527 °F | Average value: 178 °C Grade Count:63 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |