Lucite International Elvacite ® 2042 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 2042 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 2042 is a very high molecular weight ethyl methacrylate polymer. It is a tough, alcohol – tolerant, broadly compatible grade for use in abrasion – resistant coatings such as high – gloss clear lacquers for decals and outdoor signs. Slightly softer than Elvacite® 2013.Information provided by Lucite International
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
Particle Size 110 - 180 µm
110 - 180 µm
Molecular Weight 220000 g/mol
220000 g/mol
Mechanical Properties Metric English Comments
Tensile Strength 37.2 MPa
5400 psi
Elongation at Break 25 %
25 %
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 65.0 °C
149 °F
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %