Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 37.2 MPa | 5400 psi | |
Lucite International Elvacite ® 2042 Acrylic Resin Elvacite® 2042 is a very high molecular weight ethyl methacrylate polymer. It is a tough, alcohol – tolerant, broadly compatible grade for use in abrasion – resistant coatings such as h.. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | ASTM D638 |
Techmer ES Plastiblend® ABS HH BK MB Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | ASTM D412 |
Lubrizol ESTANE® 54610 Ester Based Thermoplastic Polyurethane Features: Good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion.Available in Americas, Europe, Midd.. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | ASTM D638 |
Ecomass® 1080ZD93 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing.. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Braskem D040A Homopolymer Polypropylene Description: Injection Molding, Wet and Dry Long-Term Heat AgingApplications: Suggested Uses Include Appliance, Containers, Closures, HousewaresThis resin meets the requirements for olefin polymers .. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Braskem D042M Homopolymer Polypropylene Description: Injection Molding, General Purpose, Low Water Carryover, UV ResistantApplications: Suggested Uses Include Tape, Slit-film Fibers, Containers, Closures, HousewaresThis resin meets the re.. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Braskem D080T Homopolymer Polypropylene Description: Excellent Melt Stability, General Purpose Injection MoldingApplications: Suggested Uses Include Patio Furniture, Closures, Staple FibersThis resin meets the requirements for olefin poly.. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Braskem FT120WB2 Homopolymer Polypropylene Description: Superior Antistatic properties, excellent mold release.Applications: Suggested uses include closures, housewares.Process: Injection Molding.This resin meets the requirements for olefin .. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | ASTM D638 |
Americas Styrenics STYRON® 678D High Heat Crystal Polystyrene Product CharacteristicsHigh heat resistanceExcellent clarityGood moldabilityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk organizersInfor.. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | ASTM D638 |
Aaron Industries AAROPRENE® GFIPP 2010 High Impact Glass Filled Polypropylene AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | ASTM D638 |
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet) |
|||
Tensile Strength | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Braskem D036W6 Homopolymer Polypropylene Description: Injection Molding, General Purpose, Low Water CarryoverApplications: Suggested Uses Include Tape, Slit-film Fibers, Containers, Closures, HousewaresThis resin meets the requirements for.. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Braskem H521 Homopolymer Polypropylene Description: Injection Molding, General Purpose, Low Water CarryoverApplications: Suggested Uses Include Tape, Slit-film Fibers, Containers, Closures, HousewaresThis resin meets the requirements for.. |
|||
Tensile Strength | 37.2 MPa | 5400 psi | 2 in/min; ASTM D638 |
Braskem D130C Homopolymer Polypropylene Description: High BulkApplications: Suggested Uses Include Fine Denier Staple Fiber, High Speed Fiber SpinningThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177... |