Material Notes:
Silvaloy 25 is historically a modification of Silvaloy 30 with a further reduction in silver content resulting in a higher melting point and a longer melting range. Silvaloy 25 is used for brazing steel, stainless steel, copper, copper alloys, nickel, nickel alloys or combinations of these metals. It is similar to Silvaloy 30 in performance although it contains less silver. Its broader melting range is helpful where clearances are not uniform. During melting, Silvaloy 25 passes from the solid state to a mushy or plastic state and progressively to a liquid. Typical applications are the joining of ferrous, nonferrous, and dissimilar metals and alloys with close joint clearances.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Specific Gravity 8.95 g/cc
8.95 g/cc
Density 8.94 g/cc
0.323 lb/in³
Thermal Properties Metric English Comments
Melting Point 607.2 - 746.1 °C
1125 - 1375 °F
Solidus 607.2 °C
1125 °F
Liquidus 746.1 °C
1375 °F
Maximum Service Temperature, Air 204 °C
400 °F
continuous
316 °C
600 °F
intermittent
Component Elements Properties Metric English Comments
Cadmium, Cd 12.5 - 14.5 %
12.5 - 14.5 %
Copper, Cu 35 %
35 %
Other, total <= 0.15 %
<= 0.15 %
Silver, Ag 24 - 26 %
24 - 26 %
Zinc, Zn 24.5 - 28.5 %
24.5 - 28.5 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000570 ohm-cm
0.00000570 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 710 - 843 °C
1310 - 1550 °F
Brazing Temperature
Descriptive Properties Value Comments
Color Light Yellow
Electrical Conductivity (% IACS) 29.7