Processing Properties Metric English Comments
Processing Temperature 710 °C
1310 °F
Typical Firing Temperature; Typical Firing Time: 10-15 min. at Peak
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates)
Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to..
Processing Temperature 710 - 843 °C
1310 - 1550 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® 30 Brazing Alloy
Silvaloy 30 is historically a modification of Silvaloy 35 with further reduction in silver content resulting in a higher melting point and a longer range. Silvaloy 30 is used for brazing steel, stai..
Processing Temperature 710 - 843 °C
1310 - 1550 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® A40T Brazing Alloy
Silvaloy A40T is a good general purpose, low melting, cadmium-free alloy, often selected for its low temperature, wetting and good flow. Silvaloy A40T has a lower brazing temperature with a relative..
Processing Temperature 710 - 843 °C
1310 - 1550 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy
Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manu..
Processing Temperature 710 - 843 °C
1310 - 1550 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® A50N Flux Coated Rod Brazing Alloy
Silvacote A50N Flux Cored is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nickel t..
Processing Temperature 710 - 843 °C
1310 - 1550 °F
Brazing Temperature
Lucas-Milhaupt Silvacore® A50N Flux Cored Brazing Alloy
Silvacote A50N Flux Coated Rod is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nic..
Processing Temperature 710 - 843 °C
1310 - 1550 °F
Brazing Temperature
Lucas-Milhaupt Silvacote® A50N Brazing Alloy
Silvacote A50N is a cadmium free silver brazing alloy that has found numerous applications for joining 300 series stainless steel in food, medical, and dental fields. Addition of nickel to the silve..
Processing Temperature 710 - 843 °C
1310 - 1550 °F
Brazing Temperature
Lucas-Milhaupt Silvaloy® 25 Brazing Alloy
Silvaloy 25 is historically a modification of Silvaloy 30 with a further reduction in silver content resulting in a higher melting point and a longer melting range. Silvaloy 25 is used for brazing s..
Processing Temperature 710 °C
1310 °F
Flow Temp
Wieland Porta Oprimum 710 Solder
Solder supplied as strip (0.18 oz. roll), triangular (7.09 in. rod)Information provided by WielandDental