Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 746.1 °C | 1375 °F | |
Lucas-Milhaupt Silvaloy® 25 Brazing Alloy Silvaloy 25 is historically a modification of Silvaloy 30 with a further reduction in silver content resulting in a higher melting point and a longer melting range. Silvaloy 25 is used for brazing s.. |