Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 8.95 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 8.95 g/cc
8.95 g/cc
Lucas-Milhaupt Silvaloy® A45T Brazing Alloy
Silvaloy A45T is a free flowing, low melting and an excellent substitute to the cadmium bearing filler metals with similar silver contents. Silvaloy A45T narrow melt range makes it suitable for manu..
Specific Gravity 8.95 g/cc
8.95 g/cc
Lucas-Milhaupt Silvaloy® 25 Brazing Alloy
Silvaloy 25 is historically a modification of Silvaloy 30 with a further reduction in silver content resulting in a higher melting point and a longer melting range. Silvaloy 25 is used for brazing s..