Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.65 - 1.70 g/cc
1.65 - 1.70 g/cc
ASTM D792
Filler Content 30 %
30 %
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 - 120 MPa
16000 - 17400 psi
ASTM D683
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 8.00 GPa
1160 ksi
ASTM D638
Flexural Modulus 7.00 GPa
1020 ksi
ASTM D790
Izod Impact, Notched 0.500 - 0.550 J/cm
0.937 - 1.03 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 210 - 215 °C
410 - 419 °F
ASTM D1525, HDT Method B
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
Copyright © lookpolymers.com All Rights Reserved