Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Loxim 130 01HB Polycarbonate, 30% Glass Filled, Flame Retardant

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled , Polycarbonate, Glass Fiber Filled, Flame Retardant
Manufacturer Loxim Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loxim 130 01HB Polycarbonate, 30% Glass Filled, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Loxim Industries
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Filler Content 30 %
30 %
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D1299
Mechanical Properties Metric English Comments
Tensile Strength at Break 110 - 120 MPa
16000 - 17400 psi
ASTM D683
Elongation at Break >= 2.0 %
>= 2.0 %
ASTM D638
Tensile Modulus 8.00 GPa
1160 ksi
ASTM D638
Flexural Modulus 6.50 GPa
943 ksi
ASTM D790
Izod Impact, Notched 1.30 - 1.50 J/cm
2.44 - 2.81 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
ASTM D1525, HDT Method B
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in