Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANPRO®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use.Applications: Bags for hosiery, shirts and other textiles. Food packaging for fresh fruits and produce.Advantages: Good optical properties. Excellent stiffness. High slip development and good open-ability.Fabrication: Equipment - general water quench blown film machines. Techniques - standard processing. Extrusion and water bath conditions can be varied to obtain the desired optical and mechanical film properties Information provided by Titan ChemicalsCAS# 9003-07-0
Physical Properties Metric English Comments
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Water Absorption 0.020 %
0.020 %
after 24 hrs; ASTM D570
Base Resin Melt Index 11 g/10 min

@Temperature 230 °C
11 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785A
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.67 GPa
242 ksi
ASTM D790B
Izod Impact, Notched 0.324 J/cm
0.607 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved