Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® 6331 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® 6431 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® 6531M Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® EPC40R Polypropylene impact copolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® PD701 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® PM200 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® PM201 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® PM202 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvant meet their respective FDA regulations and 21 CFR 177.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® PM383 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® PM430 Polypropylene homopolymer Titanpro® PM430 is designed without any slip agents nor antiblocking agents. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® PM655 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® PM803 Polypropylene homopolymer Titanpro® PM803 is a high flow and also a controlled rheology grade. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® SM240 Polypropylene impact copolymer Titanpro® SM240 is a high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet .. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® SM340 Polypropylene impact copolymer Titanpro® SM340 is an intermediate impact material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adju.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® SM461 Polypropylene random copolymer Titanpro® SM461 is formulated with an antiblocking and slip agents package. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® SM840 Polypropylene impact copolymer Titanpro® SM840 is an extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvant.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® SM850 Polypropylene impact copolymer Titanpro® SM850 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |
|||
Base Resin Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANPRO® SM950 Polypropylene impact copolymer Titanpro® SM950 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |