Physical Properties Metric English Comments
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® 6331 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® 6431 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® 6531M Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® EPC40R Polypropylene impact copolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® PD701 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® PD855 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® PM200 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® PM201 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® PM202 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvant meet their respective FDA regulations and 21 CFR 177..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® PM383 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® PM430 Polypropylene homopolymer
Titanpro® PM430 is designed without any slip agents nor antiblocking agents. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® PM655 Polypropylene homopolymer
The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® PM803 Polypropylene homopolymer
Titanpro® PM803 is a high flow and also a controlled rheology grade. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® SM240 Polypropylene impact copolymer
Titanpro® SM240 is a high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet ..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® SM340 Polypropylene impact copolymer
Titanpro® SM340 is an intermediate impact material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adju..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® SM461 Polypropylene random copolymer
Titanpro® SM461 is formulated with an antiblocking and slip agents package. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® SM840 Polypropylene impact copolymer
Titanpro® SM840 is an extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvant..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® SM850 Polypropylene impact copolymer
Titanpro® SM850 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The..
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Lotte Chemical Titan TITANPRO® SM950 Polypropylene impact copolymer
Titanpro® SM950 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The..