Material Notes:
MP159 is an alloy of the Multiphase family of alloys possessing the unique combination of ultra-high strength, ductility and corrosion resistance. Through work strengthening and aging, MP159 alloy exhibits ultimate tensile strength levels in excess of 265,000 psi while maintaining reduction of area values greater than 30%. Excellent strength and ductility are also evident at elevated temperatures up to 1100 - 1200 °F. MP159 alloy is produced by vacuum induction melting followed by VAC-ARC remelting to provide optimum control of chemistry and preferred ingot solidification.Information Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Density 8.33 g/cc
0.301 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 848 MPa
123000 psi
Annealed 1052°C
1590 MPa
230000 psi
Cold Worked 48%
Tensile Strength, Yield 400 MPa

@Strain 0.200 %
58000 psi

@Strain 0.200 %
Annealed 1052°C
1415 MPa

@Strain 0.200 %
205200 psi

@Strain 0.200 %
Cold Worked 48%
Elongation at Break 12 %
12 %
Cold Worked 48%
60 %
60 %
Annealed 1052°C
Reduction of Area 46 %
46 %
Cold Worked 48%
69 %
69 %
Annealed 1052°C
Modulus of Elasticity 208 GPa

@Temperature 232 °C
30200 ksi

@Temperature 450 °F
Annealed
Shear Modulus 75.8 GPa

@Temperature 232 °C
11000 ksi

@Temperature 450 °F
Annealed
Thermal Properties Metric English Comments
CTE, linear 14.3 µm/m-°C

@Temperature 25.0 - 100 °C
7.94 µin/in-°F

@Temperature 77.0 - 212 °F
14.9 µm/m-°C

@Temperature 25.0 - 500 °C
8.28 µin/in-°F

@Temperature 77.0 - 932 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.20 %
0.20 %
Chromium, Cr 19 %
19 %
Cobalt, Co 35.7 %
35.7 %
Iron, Fe 9.0 %
9.0 %
Molybdenum, Mo 7.0 %
7.0 %
Nickel, Ni 25.5 %
25.5 %
Niobium, Nb (Columbium, Cb) 0.60 %
0.60 %
Titanium, Ti 3.0 %
3.0 %
Electrical Properties Metric English Comments
Magnetic Permeability 1.00265
1.00265
At 77K