Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | >= 1590 MPa | >= 230000 psi | |
Kinetics MIM K3 Heat Treat K3 is a custom Mo-Fe alloy that provides improved fatigue properties over many other steel alloys while still maintaining good strength components, industrial or structural components and other appl.. |
|||
Tensile Strength, Ultimate | 1590 - 1600 MPa | 230000 - 232000 psi | |
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 5.75 in RCS Billet Size High Strength Alloy Steel LESCALLOY HP 9-4-30 VAC-ARC steel is a low alloy, high strength steel with a high nickel and cobalt content to promote toughness. The alloy has been designed to have high hardenability, good weldabi.. |
|||
Tensile Strength, Ultimate | >= 1586 MPa | >= 230000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 1/4 Hard, 2.5 hr at 950°F Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 2.5 hrs @ 510ºCStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation.. |
|||
Tensile Strength, Ultimate | 1586 MPa | 230000 psi | |
HP Alloys Alloy 718, 25% Cold Worked, Aged 25% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Tensile Strength, Ultimate | 1590 MPa @Temperature 316 °C |
230000 psi @Temperature 600 °F |
Tempering Temperature-800°F |
Crucible Steel 422 Stainless Steel Crucible 422 is a hardenable martensitic stainless steel which is being widely used for high temperatures up to 1200°F. It has excellent creep-rupture properties in the range of 600/1200°F and is.. |
|||
Tensile Strength, Ultimate | 1586 MPa | 230000 psi | Hardened and Stress Relieved |
AK Steel 420 Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Tensile Strength, Ultimate | 1586 MPa | 230000 psi | Hardened and Stress Relieved |
AK Steel 420 ULTRA HONE® Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Tensile Strength, Ultimate | 1586 MPa | 230000 psi | Hardened and Stress Relieved |
AK Steel 420HC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Tensile Strength, Ultimate | 1586 MPa | 230000 psi | Hardened and Stress Relieved |
AK Steel 420LC Martensitic Stainless steel AK Steel 420 provides corrosion resistance similar to Type 410 martensitic stainless steel plus increased strength and hardness. It is magnetic in both the annealed and hardened conditions. Maximu.. |
|||
Tensile Strength, Ultimate | 1586 MPa | 230000 psi | |
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Tensile Strength, Ultimate | 1590 MPa | 230000 psi | Cold Worked 48% |
Latrobe MP159® Alloy MP159 is an alloy of the Multiphase family of alloys possessing the unique combination of ultra-high strength, ductility and corrosion resistance. Through work strengthening and aging, MP159 alloy .. |