Material Notes:
Features: Antistatic, NucleatedUses: Closure Caps, Thin-walled PartsApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 112
112
ASTM D785
Tensile Strength, Yield 36.5 MPa
5300 psi
ASTM D638
Flexural Modulus 1.79 GPa
260 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Form Pellets