Material Notes:
PC/PCT alloy with good balance of physical propertiesAll information provided by LTL Color Compounders, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Melt Flow 18 g/10 min
<br>@Load 3.80 kg,<br> Temperature 260 °C
18 g/10 min
<br>@Load 8.38 lb,<br> Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.1 MPa
7700 psi
2.0 in/min; ASTM D638
Elongation at Break 150 %
150 %
2.0 in/min; ASTM D638
Flexural Strength 75.8 MPa
11000 psi
2.0 in/min; ASTM D790
Flexural Modulus 2.07 GPa
300 ksi
2.0 in/min; ASTM D790
Izod Impact, Notched 6.94 J/cm
<br>@Temperature 22.8 °C
13.0 ft-lb/in
<br>@Temperature 73.0 °F
ASTM D256