LG Chemical NBR 7030S High Acrylonitrile Polymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical NBR 7030S High Acrylonitrile Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NBR 7030S has combined the merit of NBR (Acrylonitrile rubber) with the merit of PVC resin. NBR 7030S shows good flexibility and elasticity without vulcanization, and also shows good oil resistance, chemical resistance, slip resistance. NBR 7030S can be processed and recycled like thermoplastic materials, so extrusion and injection is available and, has good flow properties so that it's possible to process at low temperature. By comparison with plasticized PVC, NBR 7030S shows good touch feeling, elasticity, anti-slip, low temperature resistance and has longer life-time by reducing the loss of plasticizer.Applications: NBR 7030S is applicable to safety shoes, fashion shoes, medical application, and hose.CAS No: 9003-18-3Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 52

@Time 15.0 sec
52

@Time 0.00417 hour
Tensile Strength at Break 10.0 MPa
1450 psi
Elongation at Break 500 %
500 %
100% Modulus 0.00608 GPa
0.882 ksi
Tear Strength 34.3 kN/m
196 pli
Abrasion 0.080

@Load 2.722 kg
0.080

@Load 6.002 lb
[cc] Akron, 3000 cycle
Thermal Properties Metric English Comments
Melting Point 150 °C
302 °F
Descriptive Properties Value Comments
Color Clear