Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 34.4 kN/m | 196 pli | post cured- 4 hours at 177°C; Die B |
Multibase SILASTIC® Q7-4735 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 34.3 kN/m | 196 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | |
LG Chemical NBR 7030S High Acrylonitrile Polymer Description: NBR 7030S has combined the merit of NBR (Acrylonitrile rubber) with the merit of PVC resin. NBR 7030S shows good flexibility and elasticity without vulcanization, and also shows good oi.. |
|||
Tear Strength | 34.4 kN/m | 196 pli | Die B |
Shin-Etsu Silicones X-30-783U Silicone Elastomer ShinEtsu X30783 U is a phenyl (PVMQ) silicone product. This product is designed for good low temperature characteristics. Product Features: A broad range of service temperatures from 100 to +260°.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Precipitated Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 34.4 kN/m | 196 pli | Notched, Die B; ASTM D 624 |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Tear Strength | 34.4 kN/m | 196 pli | Die C; ASTM D624 |
ExxonMobil Vistamaxx™ 6102 Propylene-based Elastomer Product Description: Vistamaxx 6102 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i.. |
|||
Tear Strength | 34.4 kN/m | 196 pli | Die C; ASTM D624 |
ExxonMobil Vistamaxx™ 6102FL Propylene-based Elastomer - Performance Film Product Description: Vistamaxx 6102FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | ASTM D624 |
3M Scotch® 31 Heavy Duty Mining Tape Scotch® Heavy Duty Mining Tape 31 has a tough, abrasion-resistant backing for jacket repair on mining cables. Due to extremely abrasive environment, the original jacket on the cable gets damaged of.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | ASTM D624 |
3M Scotch™ 2234 Cable Jacket Repair Tape 3M™ Scotch™ Cable Jacket Repair Tape 2234 provides a cost effective and efficient means of covering and protecting damaged sections of cable jacket, thereby extending the life of the cable and red.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 20 PHR Non-Black, Precipitated Calcium Carbonate Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Sulfur MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Suprex Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR Mistron Vapor Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 34.3 kN/m | 196 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Iceberg Clay Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |