Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical C9 Product

Category Fluid
Manufacturer LG Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical C9 Product.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties: Colorless liquid similar to DIESEL oilObtained as a by-product from pyrolysis oil hydration plant which was produced from naphtha pyrolysis process. It is composed of hydrocarbons of C9 and higher, and the content of aromatics is high.Uses: Used as a fuel for industrial boiler.Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
15.5/15.5°C
Viscosity 0.70 cP

@Temperature 100 °C
0.70 cP

@Temperature 212 °F
KSM 2014-90
1.4 cP

@Temperature 40.0 °C
1.4 cP

@Temperature 104 °F
KSM 2014-90
Thermal Properties Metric English Comments
Boiling Point 166 - 290 °C
331 - 554 °F
Flash Point 93.0 °C
199 °F
Descriptive Properties Value Comments
Autoignition Temperature 464-529°C
Components C6’s ~ C8’s Non aromatics
0.017
C8’s Aromatics
0.007
C9’s & Heavier
0.974
Styrene
0.002
Heat Value 10240-10400 cal/g
KSM 2057-92