Physical Properties Metric English Comments
Viscosity 1.4 cP

@Temperature 40.0 °C
1.4 cP

@Temperature 104 °F
KSM 2014-90
LG Chemical C9 Product
Physical Properties: Colorless liquid similar to DIESEL oilObtained as a by-product from pyrolysis oil hydration plant which was produced from naphtha pyrolysis process. It is composed of hydrocarbo..
Viscosity 1.4 cP

@Temperature 10.0 °C
1.4 cP

@Temperature 50.0 °F
Dynamic, Concentration 0.05 kg FeCl3/kg
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (2 wt% - 10 wt% Concentration)
Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene..